Stainless steel decorative plate processing to pay attention to what problems

Stainless steel color sheet

1. Stainless steel cutting tool wear (W2) is very big, especially the new workers, it’s not good to deal with, we observed the Turner the knife of time, the machine stop, between the shadow production directly, with the United States, (w) 0.8 R six sides blade, now price at RMB 38, more than 6 yuan each knife surface, the efficiency to raise 20%, down at the bottom of the technical requirements of lathe work, guarantee the quality.
2. Cooling water is very important, because in the processing of 304 heat is very high, damage to the tool, produce lumps, affect the finish, must choose stainless steel cutting liquid, the effect is very obvious.
3. For the processing of the holes, please do not be afraid to tap, (1), choose the work card of the silk work, drill bit to pay attention to the counterfeit, otherwise you will be called “huangtian”.
(2) to be sure to choose stainless steel tapping fluid, very easy, do not expect oil, paraffin oil, then you are “old”, those things in the 1970s to play.
4, the last move, for the special process requirements, cutting is difficult, choose 303 stainless steel, we used 2.5 drilling 75 deep, 304 stainless steel all scrapped, 303 phosphorus, high sulfur content, is easy to cut materials.
1. Stainless steel cutting tool wear (W2) is very big, especially the new workers, it’s not good to deal with, we observed the Turner the knife of time, the machine stop, between the shadow production directly, with the United States, (w) 0.8 R six sides blade, now price at RMB 38, more than 6 yuan each knife surface, the efficiency to raise 20%, down at the bottom of the technical requirements of lathe work, guarantee the quality.
2. Cooling water is very important, because in the processing of 304 heat is very high, damage to the tool, produce lumps, affect the finish, must choose stainless steel cutting liquid, the effect is very obvious.
3. For the processing of the holes, please do not be afraid to tap, (1), choose the work card of the silk work, drill bit to pay attention to the counterfeit, otherwise you will be called “huangtian”.
(2) to be sure to choose stainless steel tapping fluid, very easy, do not expect oil, paraffin oil, then you are “old”, those things in the 1970s to play.
4, the last move, for the special process requirements, cutting is difficult, choose 303 stainless steel, we used 2.5 drilling 75 deep, 304 stainless steel all scrapped, 303 phosphorus, high sulfur content, is easy to cut materials.

More macro prosperous stainless steel information please visit: http://www.hermessteel.net